At steam curing and moist curing conditions, the mechanical properties of concrete with different fineness and different proportions of ultrafine fly ash slag composite were studied.
研究了在蒸汽养护和标准养护条件下掺粉煤灰-矿渣复合超细粉混凝土的力学性能。
The test results show that the longer the time of moist curing, the higher the values of compressive strength, splitting tensile strength, elastic modulus and critical stress intensity factor.
试验结果表明,抗压强度、弹性模量、抗拉强度以及临界应力强度因子随标准养护时间的增长而增大,弹性模量对养护条件的敏感性最大。
No matter what it is, NSC or HSC, at the 6th day. All mechanical parameters can reach around 90% of 27 day' moist curing.
无论是NSC还是HSC,标准养护6天的力学参数都能达到标准养护27天的90%左右。